Saturday, December 18, 2010

Re: [MW:8790] ACCEPTANCE STANDARD FOR PRESSURE VESSELS

kumar,
ASME SEC IX to be followed.If your job has impact properties to be tested UG-84, ASME SEC VIII Div1 to be followed.

Regards,
Vipin

On Sat, Dec 18, 2010 at 1:35 PM, KUMAR <kumartkp@gmail.com> wrote:
Dear Sir,

In pressure vessel fabrication during welder and welding
qualification, which acceptance standard  we should follow for
mechanical test and weld visual inspection  whether ASME SEC VIII OR
IX.

--
Thanks & Regards
M.Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Vipin George

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...