Hi
 
May some cases indicate magnetism , if the ASS has been carburized or iron contaminated on the surface.
 
This can't  removable by conventional methods.
 
Thanks & Regards,
 
K. Babu
Singapore

----- Original Message -----
Sent: Friday, December 17, 2010 7:30 PM
Subject: Re: [MW:8778] RE: 0] How to remove magnetism from SA240 TP 304 L material.

Try passing AC thru it from a welding machine and reducing the current gradually to zero. Not so sure about Aust SS (I mean the reason, may be there is some other phase present or cold working could have introduced some dipoles...), but this has worked on other non Aust SS quite well. For all practical purposes, you need to lower residual magnetism  down to <6G. Heating was another method for non-Aust SS, which you say did not work in this case...

--- On Fri, 17/12/10, Kisan Gamane <kisankrishna1506@gmail.com> wrote:

From: Kisan Gamane <kisankrishna1506@gmail.com>
Subject: Re: [MW:8773] RE: 0] How to remove magnetism from SA240 TP 304 L material.
To: materials-welding@googlegroups.com
Date: Friday, 17 December, 2010, 3:05 PM

Dear Pablo
We have using this material in energy equipment. In plate form it shows slight magnetism ; But we have not its exact value. But this magnetism varies the end users electrical parameter. Hence we require the solution to remove  magnetism. we have already done solution analing at 1050 Deg. Celcius.


 
On Fri, Dec 17, 2010 at 2:48 PM, C<pjacelajado@npc.com.sa> wrote:

Hi!

 

TP304L is an austenic stainless steel. If there is magnetism, what is the value in Gauss or in Tesla? 

 

Thanks.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kisan Gamane
Sent: Friday, December 17, 2010 11:11 AM
To: materials-welding@googlegroups.com
Subject: [MW:0] How to remove magnetism from SA240 TP 304 L material.

 

Dear All

Anybody can tell how to remove magnetism from SA240 TP 304 L material.

 

Thanks & regards

--

किसन गामणे

नाशिक

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

किसन गामणे

नाशिक

जन्मलो म्हणून जगणार नाही
अन असाच राखेत विरणार नाही...
ठसे सोडूनी जाईन जीवन काठावरती
आल्या लाटा कितीही , मिटणार नाही ...

 

खुभी नाही माझ्यात एवढी  कि..!
कुणाच्या  हृदयात ठाण  मांडून  जाईल..!
पण विसरणे सुद्धा अशक्य होईल..!
असे  क्षण  देऊन जाईल.......!

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...