Wednesday, December 15, 2010

Re: [MW:8747] PWHT for Stelliting on WC9 Material

Its as per your wps requirement and the required hardness. Please consult the electrode supplier or its data sheet.

2010/12/15 Muni Andy <cmkfc07@gmail.com>
What is the recommended Post Weld Heat treatment Temperature for hardfacing overlay on WC9 material?
Which standards cover this details?
C.Muniyandi
Coimbatore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...