Pipe thickness (i.e. schedule) is derived for the design pressure it is supposed to withstand. BAsed on design pressure hydrotest pressure is worked out. It is never vice-versa.
However you can work out the maximum test pressure using Specified Minimum Yield strengh (SMYP) of the pipe in question and use 90% of this value for calculation of test pressure.
----- Original Message -----
From: prabhu duraisamy
To: materials-welding@googlegroups.com
Sent: Tue, 14 Dec 2010 21:43:13 +0530 (IST)
Subject: [MW:8731] SS Pipe Hydrotest Pressure rating chart
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
However you can work out the maximum test pressure using Specified Minimum Yield strengh (SMYP) of the pipe in question and use 90% of this value for calculation of test pressure.
----- Original Message -----
From: prabhu duraisamy
To: materials-welding@googlegroups.com
Sent: Tue, 14 Dec 2010 21:43:13 +0530 (IST)
Subject: [MW:8731] SS Pipe Hydrotest Pressure rating chart
Dear Friends,
Can you please explain to me, what is the min. Hydro test pressure limit of A312 TP316/316L Seamless pipe 2" to 6" Sch.40 & Sch80.
Thanks
D.Prabhu
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments