Manpreet :
I refer to ASME B16.34 (Pipeline Transport System) to answer your question below :
Par 437.1.4 Testing After New Construction .
1. System to be operated at a hoop stress of more than 20 % of the specified minimum yield strength of the pipe shall be hydrostatically tested
2. System to be operated at a hoop stress of less than 20 % of the specified minimum yield strength of the pipe may be subjected to leak test
Regards, Bonardo
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
I refer to ASME B16.34 (Pipeline Transport System) to answer your question below :
Par 437.1.4 Testing After New Construction .
1. System to be operated at a hoop stress of more than 20 % of the specified minimum yield strength of the pipe shall be hydrostatically tested
2. System to be operated at a hoop stress of less than 20 % of the specified minimum yield strength of the pipe may be subjected to leak test
Regards, Bonardo
2010/12/13 manpreet <manpreetsin88@rediffmail.com>
Dear All,
Can someone help me to find when is it required to hydrotest parts in pipeline, Please provide information in detail, with code reference (if possible AS2885). I am aware Pressure vessel require Hydrotest, but it's not clear for pipeline.
Any information would be much appreciated.
Regards
Manpreet Singh
Welding Engineer--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments