Re: [MW:8659] normalizing temperature requirement

Dear Asad,

You will have to select the normalizing temperature using Iron-Carbon diagram based on the carbon content of the material.

Arunachalam.A

On Thu, Dec 9, 2010 at 1:06 PM, asad azmi <azmiasadayub@gmail.com> wrote:
dear all,
 
Greetings.
 
please inform me what is the minimum and maxiumum Noramlizing  Soaking temperature and Saoking time for material SA 387 GR 12 CL2, 70 THK.
 
what will be the maxium temeperature  for hot forming of dished head   for the above material. will it be same as Normalizing temperature or different.
 
please give code reference.
 
Regards
 
Asad Azmi
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...