Hi
Are you talking about max. Fe (iron) content ?
Ferrite content in overlay of Inconel 625 deposit ???
How much is the required overlay thickness ?
Please clarify...
Regards
Prem Nautiyal
On Wed, 08 Dec 2010 12:30:02 +0530 wrote
>Dear All,
I've got a doubt on the following issue,
We're going to make an overlay with INCONEL 625 over SA 516 Gr. 70
(60mm thick) on its edge. But when we do the PQR for this the ferrite
content on this overlay is found to be 4%. Is there any standard
restricting this??? Because my client is asking for a max. of Ferrite
content of 3%.
Please Reply.
Regards
Akhil
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
PREM S NAUTIYAL
CELL : 9769316004
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Are you talking about max. Fe (iron) content ?
Ferrite content in overlay of Inconel 625 deposit ???
How much is the required overlay thickness ?
Please clarify...
Regards
Prem Nautiyal
On Wed, 08 Dec 2010 12:30:02 +0530 wrote
>Dear All,
I've got a doubt on the following issue,
We're going to make an overlay with INCONEL 625 over SA 516 Gr. 70
(60mm thick) on its edge. But when we do the PQR for this the ferrite
content on this overlay is found to be 4%. Is there any standard
restricting this??? Because my client is asking for a max. of Ferrite
content of 3%.
Please Reply.
Regards
Akhil
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
PREM S NAUTIYAL
CELL : 9769316004
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com