Dear Saeed,
As per Code Case 2235 UT instead of RT is acceptable for Thickness greater than 13mm.In ASME Sec VIII Div 2 2010 edition code case is part of code.You can do either TOFD or Phased array.Both Tofd or Phased array is better than RT in case of higher thickness.
--
With Warm regards,
G.Padmanabhan
+96895685853
-- As per Code Case 2235 UT instead of RT is acceptable for Thickness greater than 13mm.In ASME Sec VIII Div 2 2010 edition code case is part of code.You can do either TOFD or Phased array.Both Tofd or Phased array is better than RT in case of higher thickness.
On Tue, Dec 7, 2010 at 1:30 PM, Navid Navidi <navid_751400@yahoo.com> wrote:
--Hi all,
is it possible to use phased array technique instead of RT for NDT teast of a pressure vessels.
Does standard allow us to do so?
what is its advantages?
thank you in advance
Saeed
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
With Warm regards,
G.Padmanabhan
+96895685853
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment