Good morning Mr.Navid,
ASME have code case 2235 ,this code case saying we can use recordable UT in replace of RT,
& phase array is a recordable UT,so for me it is acceptable.but please take advice form AI if the vessel is code stamp.
please refer code-case 2235 latest revision.
--
Thanks & Regards.
Santosh Gaikwad
Material Testing & Inspection Services(MTIS),
Surat,India.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
ASME have code case 2235 ,this code case saying we can use recordable UT in replace of RT,
& phase array is a recordable UT,so for me it is acceptable.but please take advice form AI if the vessel is code stamp.
please refer code-case 2235 latest revision.
--
Thanks & Regards.
Santosh Gaikwad
Material Testing & Inspection Services(MTIS),
Surat,India.
On Tue, Dec 7, 2010 at 9:00 AM, Navid Navidi <navid_751400@yahoo.com> wrote:
--Hi all,
is it possible to use phased array technique instead of RT for NDT teast of a pressure vessels.
Does standard allow us to do so?
what is its advantages?
thank you in advance
Saeed
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.