Friday, December 17, 2010

[MW:8766] Er-NiCu-7 composition

hello all;

we have D&H electrodes Er-NiCu-7 supplied with following composition
C=0.005
Fe=0.65
Si=0.18
Al=0.032

Any problems accepting this as these elmnts are falling short of range
though below maximum specified as per AWS5.14??

YOGESH

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire