dear all,

depends on the repair if in root (IF, LOP) due to hi-low or missmatch
especially fittings, it is prefferred to cut out and re fit up makes
more tappering inside the pipe fittings to be match the inside dia.
but make sure that is performed properly atleast 30 deg. angle of
tapper.

marcelo p soriano
qa/qc eng'r.

On Dec 5, 7:04 pm, "cyril andrews" <jcyriland...@gmail.com> wrote:
> Dear All,
>
>    Here I have a doubt regarding 2"pipe welding . While  work with 2" pipe,
> if repair comes and founded in Rt. What we have to do as per ASME SEC VIII
> Div.1. I found one company is doing partial repair and taking Partial RT.
> Whether it is correct? I couldn't conclude with this. Please suggest a good
> answer.
>
> J.C.Andrews,
>
> QA/QC Engineer,
>
> Doha-Qatar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...