Friday, December 3, 2010

[MW:8499] REGARDING STAINLESS STEEL(304L) Welding

Dear all,
 
 
WE ARE USING STANLESS STEEL 304L(THCKNESS-4mm) FOR TANK FABRICATION WITH MAG PROCESS.WITH AUTOMATIC WELDING .
 
KINDLY SUGGEST ME WHAT WILL TE SHIELDING GAS,PURING GAS & FILLER WIRE.
 
ANY PWHT REQUIREMENT FOR THIS WELDING.

--
Regards,
Pushpraj Anand


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point