dear desai
No problem for low temp service ,both materials fall on curve C,with Supp.req S2 you may go for low temp .
regards
yogesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No problem for low temp service ,both materials fall on curve C,with Supp.req S2 you may go for low temp .
regards
yogesh
On Mon, Nov 15, 2010 at 10:39 PM, Dhwani Desai <dhwani0608@yahoo.com> wrote:
--
Dear Members,
In general, we all know based on description given in ASTM of A671 & A672 that A671 is used for atm. & low temperature service & A672 for H.P. service at moderate temperature.
However, if we compare the details e.g. A672 Gr.C60 & A671 Gr. CC60; the raw material plate used is same for both pipes & final mechanical properties is same.
Heat treatment is same.
Can any one explain or comment if A672 Gr.C60 with Suppl. req.S2 can be used for Low temp. service & why?
Dhwani Desai
Planning & Piping Dept.
Ext.-7681
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments