[MW:8267] PWHT and RT

Hi,

I have a doubt regarding PWHT and RT. We are welding P1 Material Pipes which has thickness more than 19mm so we are performing PWHT for the same. But my question is regarding when to take RT? Can we accept the joints which is radiographed before PWHT and  MPI after PWHT. Or will we have to perform the RT only after PWHT of the joints? Please advice me regarding this and provide the supporting clause.

Thanks and Regards,
Sagar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...