Zul,
Position of welding is not a Essential variable for Procedure
qualification ie you can use the WPS for any position .in case of
welders qualification it is essential variable.
Your WPS can be used for 1G with the PQR qualified in 3G.
In general practice the welder who welds PQR test piece is also
qualified hence we are qualifying in 6G position to enable welder
qualification in parallel with PQR
regards,
vaithiyanathan
Position of welding is not a Essential variable for Procedure
qualification ie you can use the WPS for any position .in case of
welders qualification it is essential variable.
Your WPS can be used for 1G with the PQR qualified in 3G.
In general practice the welder who welds PQR test piece is also
qualified hence we are qualifying in 6G position to enable welder
qualification in parallel with PQR
regards,
vaithiyanathan
On Nov 11, 1:35 pm, Zulfan <zul...@insing.com> wrote:
> Dear all,
>
> please advice in our PQR mentioning position 3G and our WPS stated 1G
> is the WPS able to apply or need to run again PQR again?
> code ASME sec IX
>
> Thank
> zul
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments