Dear members,
I've a question about Macro examination in
PQR's. What is the minimum magnifcation level we need to have? ,is
there any reference standard/specification .
One of my client spec syas it must be x5 .I have come across with
various PQR review this magnification level is varying a range from
x2.7 ,x3.4,x4.0&x5.0.
I've a question about Macro examination in
PQR's. What is the minimum magnifcation level we need to have? ,is
there any reference standard/specification .
One of my client spec syas it must be x5 .I have come across with
various PQR review this magnification level is varying a range from
x2.7 ,x3.4,x4.0&x5.0.
Also is there any significance in referring the letter in small
case(x5) or Caps(X5)
Any one can put your expertise in this regard.
pavainathan
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments