Tuesday, November 2, 2010

[MW:8017] Accelerated Cooling of A517-Gr.B and its Post-heating

Dear all,

Can we do accelerated cooling by air a A517-Gr.B weldment from its stress relief
temperature (540-590°C)? Is there any necessity for post-heating of A517-Gr.B after welding?
 
Thanks
 
Kianoush Zarrin naghsh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...