Dear Friend,
 
A333  LTCS,its Al killed chemical properties,impcat value is conformed.
if other than more,please let me know about this.
thanks and regards
Sujay

On Tue, Oct 26, 2010 at 9:31 AM, Martin Prad <martin_prad@hotmail.com> wrote:
Hi,
 
What is the real difference of ASTM A333 pipe from ASTM a106grB?
ASTM A333 is a low temperature CS pipe but 106 is not. What is the main features of Low temperature CS steel pipes by their chemical composition and mechanical properties?
Please share your experience on this.
 
Martin.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...