Re: [MW:7643] Change in electrode manufacturer

Hi
If your code is ASME Sec. IX, You can use as it is identifiable with the A no.
If A no. is not applicable then you have to prove for same chemical composition or restrict with the same brand as PQR.
Thanks and Best regards,
K.Rajagopal
On Tue, Oct 19, 2010 at 8:15 AM, krishna <wiqw@rediffmail.com> wrote:
Hi frnds,
Please clarify the below

we have qualified a welding procedure with ESAB E07018 and it is passed we are doing the production welding .

Now we have no stock of ESAB so we are using HONAVAR Electrodes with the same WPS.

Is it acceptable or we have to make another procedure with honavar electordes.

regards,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Blog Archive