Re: [MW:7614] Normalizing of Weld joints

Generaly with soaking time of 1 minute per mm and max of 1 hour at 900 c. We can achieve acceptable UTS of weld of gr 70 plate up to 50 mm thk. However. For higher thk weld it is difficult to achieve UTS in such case better to use consumable having higher Mn

For such case we need to qualify ,
NR + SR. To estblish the result we need to have simulation
Regards
Hegde

Sent from my BlackBerry® smartphone from !DEA


From: "Vanchinath S.A." <vanchinaths@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Sun, 17 Oct 2010 19:08:35 +0530
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: Re: [MW:7611] Normalizing of Weld joints

normalising temp should be in the range of 880 to 920 degC and soaking time 1/2 hr per inch thk. higher soaking time will result in lowering of weld strength.
vanchi

On Sat, Oct 16, 2010 at 5:40 PM, pavainathan <pavainathan@gmail.com> wrote:
Hi Memebers,
                     We have welded fitting (A 234 WPBW) which needs
to be Normalized after welding around temeperature 825 DegC .I look
for some specification reference to calculate the soaking time for the
thickness range 20-25mm . Any one can suggest me the options.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...