There is no limit as per code for electrode weaving, its only mentioned in some clients specifications.
 


 
On Sat, Oct 16, 2010 at 6:02 AM, limesh M <limesh78@gmail.com> wrote:
Dear All,
 
I heard about weaving ,which is applicable in SMAW.If I am crossing the weaving barrier as per manufacturer recommendation,ie,  2.5 X dia of electrode or 3 X dia of electrode what would happen?
 
Is weaving applicable in GTAW? If applicable what would be the weaving range?
 
 
 
Regards,
 
Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,

S.Tulasi Ramu
+971 50 8175303 ( Abudhabi), +91 9866998074(India).

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...