Re: [MW:7595] Purge Gas

Leave it to 8mm min
A


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Sent: Sat Oct 16 06:14:09 2010
Subject: [MW:7587] Purge Gas


When can we remove backing gas purge from non-ferrous pipe joints.
Can we remove the gas purge once the root run is complete, or once the root and first hot pass is complete.
We leave the gas purge on until the joint is capped and i am sure this is wasting gas.
John Hardcastle
 
Fabrication Manager

Euro Mechanical Contractors Company Factory
P.O. Box 46153
Abu Dhabi
United Arab Emirates
 
Phone: +971 2 550 08 99
Fax: +971 2 5501898
Mobile: +971 50 4445873
 
Email: jhardcastle@euromechanical.com
www.euromechanical.com



This email is intended for the addressee(s) only, and may contain confidential or privileged information. Unauthorised use of this information, or distribution, copying or other dissemination is strictly prohibited.

If you have received this email in error, please destroy it immediately.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 ************************************************************************* This e-mail message and any attachments to it are intended only for the  named recipients and may contain confidential information. If you are not one of the intended recipients, please do not duplicate or forward this e-mail message and immediately delete it from your computer. If you  received this email in error, please notify postmaster@veoliawater.com *************************************************************************       

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...