Thursday, October 14, 2010

Re: [MW:7572] EN10204 3.2 certification

Applicable for pressure part of Pressure Vessel. But Over all pressure vessel its not applicable.

Its specific client requirements.some client requirements EN 10204 type certificate.


Regards,
Vikas Rana



On Thu, Oct 14, 2010 at 8:28 PM, Ravi Karuskar <rkaruskar@gmail.com> wrote:
For pressure vessel also possible in 3.2 certification.

Ravi Karuskar

On 10/14/10, limesh M <limesh78@gmail.com> wrote:
> Dear Aarpee,
>
> I don't know how to interpret,but one thing I can say,3.2 certification is
> applicable to valves based on customer requirement(In our current project we
> are purchasing valves with 3.2 certificates).3.2 certification on Pressure
> vessels,hmmm,I don't know.Seniors advise is required.
>
>
> Regards,
>
> Limesh
>
> On Thu, Oct 14, 2010 at 10:58 AM, Aarpee <ramprasad.chari@gmail.com> wrote:
>
>> Dear all,
>> Can 3.2 certfication be applied to Valves and Pressure vessels OR can
>> 3.2 certification be applied to "assembled' and "welded" products?
>> This query is due to scope defined in the standard as:
>> "This document specifies different types of inspection documents
>> supplied to the purchaser in accordance with the requirements of the
>> order,for delivery of all metallic products e.g
>> plates,sheets,bars,forgings,castings,whatever their method of
>> production"
>>
>> I wish to have your views/interpretation/experience on above.
>>
>> Regards
>> Aarpee
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding-unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Ravi Karuskar
Trelleborg Marine Systems India Pvt. Ltd.,
Akik,Bodakdev, S.G.Highway, Ahmedabad
Mob. 9727802502
Email : rkaruskar@gmail.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...