Hi
 
May i know is it needed to kept overnight in oven in 150 degreee celsius.?
I think tat just before 2hrs before any job is enough?
Pl cleare me....
 
Thanks
m

On Tue, Oct 12, 2010 at 8:07 AM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Vasu,
 
Pls find below as my opinion,
 
Regards,
 
K.Babu
 
----- Original Message -----
From: vasu k
Sent: Tuesday, October 12, 2010 1:18 AM
Subject: [MW:7486] reg baking

Dear All,

Iam new to piping. I have some basic doubts and i request you to please clarify..

1. In our fab yard, in the evening after the work is finished, the remaining electrodes(E-7018 and E-7018-1) are being kept back in the oven and the entire night the oven will be at 150 deg.
    Will it affect the coating if they r kept for that much time (the entire night)?
No

2. Do i have to do baking for those electrodes again in the morning?
 
Not Required

3. What is the max number of recycling of electrodes?
 
Re-Baking maximum of only once

4. what is the purpose of doing baking till 250 deg ?
 
Removal of Adsorbed moiture
 
doesnt the moisture will be removed if we maintain 150 deg i.e  continuously at holding temp?
Mfg has to advise

Regards,

vasu.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...