Skip to main content

Re: [MW:7458] difference between tightening test and tightness test in piping work.

Please refer to ASME PCC-01, GUIDELINES FOR PRESSURE BOUNDARY BOLTED FLANGE JOINT ASSEMBLY for guide lines.

arun

2010/10/7 César Alexis Viteri Pérez <alexis_viteri@hotmail.com>
Dear Mr. Dilip,,
 
Sometimes when u have to do a Tie in, bolt tightening doesn't  guarantee abscense of leaks because of bolted spools can´t be perfectly fitted, then some clients requieres a leak test prior to comissioning the facility.
 
BR
Alexis

Date: Wed, 6 Oct 2010 22:25:39 -0700
From: karthik6684@yahoo.com
Subject: Re: [MW:7409] difference between tightening test and tightness test in piping work.
To: materials-welding@googlegroups.com

Dear Mr.Dilip,
As per B31.1,Section 137.1 - The tightness test is a pressure test as required by code and it shall be done after all NDE and PWHT work finished.The pressure testing of the piping systems is to ensure the leak tightness shall be acceptable for the determination of any leaks in piping sub assemblies.
 
AS per your quiery,i understood that you are doing Initial Service test.But the Initial service test is normally specified by some customer.If your customer specify for Initial service test,please follow,ASME B31.1,Section 137.7.
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Thu, 10/7/10, ctcit-an&mma-Dilip Kumar <dilipkumar@ctci.co.th> wrote:

From: ctcit-an&mma-Dilip Kumar <dilipkumar@ctci.co.th>
Subject: [MW:7407] difference between tightening test and tightness test in piping work.
To: materials-welding@googlegroups.com
Date: Thursday, October 7, 2010, 10:49 AM

Dear Friends,

 

We have a situation where we saying the tightening test is a process of bolt tightening only, but the tightness test is the activity to be performed after completion of re-instatement of piping work (after flushing cleaning and before commissioning) by putting the medium (air, water etc.) inside the piping work and perform the leak test for all the mechanical joints.

 

Any advice will be appreciated and if have some supporting documents/code to support above mention understandings.

 

Thanks

 

With regards.

 

DK.

 

P  Note- Please consider the environment before printing this e-mail.

  --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...