Dear Devarajan,
 
May i know induction coil heating is it same as Electrical resistance heating for PWHT,
 
Thanks

On Mon, Oct 4, 2010 at 1:18 PM, Devarajan Ramasamy <neo.devarajan@gmail.com> wrote:
For any preheating more than 150 deg C, induction coil heating is much preferred. 


On Mon, Oct 4, 2010 at 4:53 PM, Engineer Mech <mengineer010@gmail.com> wrote:
Dear All,

Job is Bush & Shaft welding,
Shaft is about 300 mm OD, Preheating is 220 degree celsius
By which way i can do preheating, Heating torch is enough for
preheating of this job, or Electrical resistance heating is it need to
do?
I think Heating torch is ok!
Pl clear me...

Regards
M

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
This message originated from the Internet. Its originator may or may not be who they claim to be and the information contained in the message and any attachments may or may not be accurate.

This email transmission is intended solely for the named recipient(s). It may contain confidential and/or privileged information.If you are not the intended recipient, note that disclosing, copying or distributing it may be unlawful. Please notify the sender immediately if you have received it by mistake, and delete it from your system.
Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.

"SAVE PAPER - THINK BEFORE YOU PRINT!"

Regards,

~ DEVARAJAN RAMASAMY~

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...