Re: [MW:7339] Pneumatic test not réalised at shop

Hello my friends,

Thank you very much for your answers.

I consulted the ASME B31.3 code  "vent hole" for reinforcement and I found this  article 328.5.4 connections ( g ) and ( h ) page 64 edition(publishing) 2008.

 

G) Reinforcing pads and saddles shall have has good made with the parts to which they are attached. In wind hole shall be provided at the side (not at the crotch) of any pad now saddle to reveal leakage in the weld between branch and run and to allow venting during welding and heat treatment. In pad now saddle may be made in more than one piece yew joints golden between pieces have strength equivalent to pad saddle relative(parent) metal, and each piece has yew has wind hole.

H) Examination and any necessary repairs of the completed weld between branch and run sh has pad now saddle.

 

If I apply this article what is that the pneumatic test will be applied or the fluorescent penetration test ?

My best regards

Redouane (Project engineer)

Algeria



2010/10/1, parviz farhadi <parvizfarhadi@gmail.com>:
One thing that remembered that may related to this is, in prevoius project our contractor was doing PWHT for a portion of pipe that reinforced pipe was near it and in that pad there was not tell tale hole or weep hole, and this made finally a blast in that pad, which was very dangerous, just lucky that nobody injured.

On Fri, Oct 1, 2010 at 12:34 AM, Brl Pp <refazosaris@gmail.com> wrote:
My friends,

Good morning,

There is somebody who can give me advice concerning the pneumatic test
not realised by my contractor (in the shop).

It is about spools of various diameters the biggest diameter is 60''.

The product is the liquefied natural gas (LNG).

My contractor realized a big party of spools painted without the
pneumatic test of the reinforcements and sent on the site.

Please, how I am going to make.

Thank you in advance and good luck

Redouane (Project engineer)

Algeria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...