Re: [MW:7311] Pneumatic test not réalised at shop

One thing that remembered that may related to this is, in prevoius project our contractor was doing PWHT for a portion of pipe that reinforced pipe was near it and in that pad there was not tell tale hole or weep hole, and this made finally a blast in that pad, which was very dangerous, just lucky that nobody injured.

On Fri, Oct 1, 2010 at 12:34 AM, Brl Pp <refazosaris@gmail.com> wrote:
My friends,

Good morning,

There is somebody who can give me advice concerning the pneumatic test
not realised by my contractor (in the shop).

It is about spools of various diameters the biggest diameter is 60''.

The product is the liquefied natural gas (LNG).

My contractor realized a big party of spools painted without the
pneumatic test of the reinforcements and sent on the site.

Please, how I am going to make.

Thank you in advance and good luck

Redouane (Project engineer)

Algeria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...