Re: [MW:7308] Pneumatic test not réalised at shop

Dear Frtiend,
                      Regarding to your Question, please refer ASME B31.1 for your answer. it is clearly mentioned that you can replace pressure test to non destructive testing if you are not performrd prssure test during manufacturring. RT all joints 100% u have the subsituite.
 Regards.
Ehtisham Farooq,
Inspection Engineer,
BUreau Veritas Pakistan.


From: Brl Pp <refazosaris@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Fri, October 1, 2010 11:34:34 AM
Subject: [MW:7301] Pneumatic test not réalised at shop

My friends,

Good morning,

There is somebody who can give me advice concerning the pneumatic test
not realised by my contractor (in the shop).

It is about spools of various diameters the biggest diameter is 60''.

The product is the liquefied natural gas (LNG).

My contractor realized a big party of spools painted without the
pneumatic test of the reinforcements and sent on the site.

Please, how I am going to make.

Thank you in advance and good luck

Redouane (Project engineer)

Algeria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...