Dear,
 
In process pipe work normally GTAW,SMAW and SAW are preferred.It doesn't mean that GMAW is forbidden.But many clients not much interested in GMAW process on their pipe work due to it's poor performance history.But one reputed main contractor approved this process(Automatic GMAW) for root and hot pass welding for thin walled mega bore(one person can easily walk through) carbon steel pipes for their air seperation Unit project.RT result of the welded joint was poor. Welding contractor's QC has no time to sit inside his office.Luckily I got a chance to see all defects (Thanks to God and the main contractor,It was a good experience for me).The thin walled pipes fit up was the major problem,even the mismatch goes upto 6 mm.The same process was used in heavy walled CS pipe spool fabrication in another project and the radiography result was good.In this case the fit up was too good.
 
 GMAW - Handle with care especially in pipe work.
 
Regards,
 
Limesh
On Thu, Oct 14, 2010 at 11:54 AM, Clubb, Archie <Archie.Clubb@veoliawater.com> wrote:

All

 

Agree with Karthic – the use of GMAW and FCAW are simply to speed up and cheapen the work ! – Bang goes the quality – Stick to the TIG as far as possible at roots.

 

 

 

Archie

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of hany alfy
Sent: 14 October 2010 06:26

Subject: Re: [MW:7547] GMAW instead of GTAW +SMAW

 

You can use GMAW no problems

Use Metalloy Wires it is give good reuslts with the proper WPS/PQR

for CS Pipes u can use Metalloy 76 i attached the data for you here (Before it was Metalloy 71)

if u need any more pls contact me

Hani Alfe

 


From: Karthik <karthik6684@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Thu, October 14, 2010 8:08:22 AM
Subject: Re: [MW:7544] GMAW instead of GTAW +SMAW


Hi,

Normally GMAW is not allowed in piping and pressure vessel welding because of the more weld defects even which cannot identify in RT.

But With proper application and appropriate parameters, excellent welds can be produced using short-circuit GMAW.  However, if the welder is not careful to follow established procedures, a number of serious weld defects can occur.

The most significant of these defects is lack of sidewall fusion; the molten puddle of metal does not fully fuse with the pipe sidewalls, and a "cold lap" defect occurs.  This is a significant structural defect that is difficult to identify with commonly used nondestructive inspection methods such as radiography.  So while the GMAW and FCAW processes have gained popularity for many applications, they have not been considered serious options for most pipe welding operations.

This poor reputation is no longer deserved, however.  Continuous development in both power supply and consumable technology have made this process a viable alternative to manual GTAW or shielded metal arc welding (SMAW) of pipe.

Thanks & Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager

Getabec Energy Co.,Ltd.

379,Moo6,Soi8,Nikhomphatana,

Rayong-21180,

Thailand.

Phone: 0066 38 897035-8 (Off)

Fax: 0066 38 897034

Hand Phone: 0066 892512282



--- On Thu, 10/14/10, rupeshjambhale@gmail.com <rupeshjambhale@gmail.com> wrote:


From: rupeshjambhale@gmail.com <rupeshjambhale@gmail.com>
Subject: [MW:7543] GMAW instead of GTAW +SMAW
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Thursday, October 14, 2010, 10:50 AM

Our contractor want to use GMAW process inplace of GTAW+SMAW
for cS pipe butt weld joint. Construction code is B31.3  . Can we quaLify OR use GMAW  inplace of Gtaw+ smaw process. Pressure is 15 kg/cm2g with full RT. Pls advice?bscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



     

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

***************************************************************************************************************************************************************************
This e-mail (which includes any files attached to it), it is intended solely for the named recipient and may contain CONFIDENTIAL, legally privileged or trade
secret information protected by law. It has been sent it via the internet and is therefore not secure against corruption, interception or unauthorised modification.

If you are not the intended recipient please do not read, use, disclose, distribute, copy, print or rely on any information contained in this e-mail. Please
immediately notify us by telephoning +44 (0) 1494 887808 or return it to us by e-mail to the sender, confirming that this e-mail has been deleted from
your system and any hard copies destroyed.

To the extent permitted by law, neither we nor any of our subsidiaries, parent entities or other affiliates, nor any employee, director or officer thereof,
accepts any liability whatsoever in relation to this e-mail including liability arising from any external breach of security or confidentiality or for virus
infection or for statements made which are clearly the sender's own and not made on our behalf.

"We" and "our" in this footer refer to the following legal entity:

VWS Westgarth Ltd. Registered in Scotland No. 147604, Orbital House, 3 Redwood Crescent, East Kilbride, G74 5PR

This company is a member of the Veolia Water Solutions & Technologies group, but please contact the sender should you have any question
regarding the legal entity on whose behalf this email was sent.
***************************************************************************************************************************************************************************

************************************************************************* This e-mail message and any attachments to it are intended only for the  named recipients and may contain confidential information. If you are not one of the intended recipients, please do not duplicate or forward this e-mail message and immediately delete it from your computer. If you  received this email in error, please notify postmaster@veoliawater.com *************************************************************************       

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...