Sunday, October 24, 2010

[MW:7762] Separation of joint

Dear All,
 
During fit-up of two spools of SS304, It was observed that logitudinal seams of pipe are coming face to face, means there is no separation between long seams of large dia pipe. Is there any criteria stated in asme B31.3  or Aramco standard in this regard.
 
Regards,
 
Ahmed H.
 

 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...