Thursday, October 21, 2010

[MW:7693] Re: Beginning to SA-450 meaning

Pls Refer- UG 81, Over crowining 1-1/4% of ID and Under crowining 5/8%
of ID.

Regards
Israr Ahmed(Surveyor)
Tata Projects Ltd.
+919930308261


On Oct 21, 10:40 am, vijay panchal <panchalvijay...@gmail.com> wrote:
> PLS can u tell me that how much overcrowing is permissible in 2:1
> ellispodial dishend and trospherical and in section vii Where to refer
> pls its urgent i need u r help
>
>  thanks
> vijay
>
>
>
> On Tue, Oct 19, 2010 at 7:14 PM, limesh M <limes...@gmail.com> wrote:
> > *Dear All,*
> > **
> > *I found that,Beginning to SA-450 on the front page of ASME BPV SEC II
> > Part A 2010 Edition.What it means? *
> > **
> > **
> > *Regards,*
> > **
> > *Limesh*
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding-unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.- Hide quoted text -
>
> - Show quoted text -

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...