Hi
API 572 : Clause-10.3.9
Recommended resistance is 5 ohms or less, and resistance is not to exceed 25 ohms.
Which valuse we need to consider ?
Thanks & Regards,
K.Babu
Singapore
Singapore
Hello, Please see the response below. Regards. P. Goswami, P. Eng, IWE. From: materials-welding@googlegroups.com <materials-weld...