Wednesday, October 13, 2010

[MW:7526] x-ray in the shop

good morning,

can I use X- ray for below 8mm class IV caron steel and stainless
steel piping in the shop?

what means AGFA D5, AGFA D4/D2?

please shar your exerience

my regards

redouane

--