Hello Mr. Philip,

You can ask your lab to certify the test as per ASME Sec IX and AWS
D1.1 and you can prepare separate WPS as per Sec IX and D1.1 and use
the same test to prepare PQR then you can use the qualified WPS as per
ASME and AWS D1.1.

I have done the same while i was there in Dubai and same was accepted
by ABSG.

On Sep 28, 5:00 pm, "Philip, Taiye (Lagos)"
<Taiye.Phi...@deltaafrik.com> wrote:
> Hello gents,
>
>  I have a WPS qualified as per D1.1 - 8 inches for welding structural
> work, in 6G position,
>
> My query is can I use these procedure to weld pipe work as per ASME IX
> for the same material?
>
> Pls I need further clarification with codes support.
>
> Regards
>
> Philip Taiye
>
> *** WORLEYPARSONS GROUP NOTICE ***
> "This email is confidential.  If you are not the intended recipient, you must not disclose  or  use the  information contained in it.
> If you have received this email in error,  please notify us immediately by return email and delete the email and any attachments.
> Any personal views or opinions expressed by the writer may not
> necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...