I want to Qualify a PQR in pipe  Material LTCS-A333Gr6.Pipe Dia is 8".
 
now my Question is for Destructive test (IMPACT) ,from which location I have to cut?
 
please give ASME reference also.

Girish K. Vora
09978910870

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

1 comment:

Unknown said...

Please specify welding position. Please refer to QW463.1(d) or (e) or (f) ASME SECIX 2007.