Friday, October 1, 2010

[MW:7312] RE: 7290] Electrode for cast steel

Larry,

Using pre-heat, stress relief peening, and post heat, this is the best product by far

http://www.rockmountnassau.com/product1.html

 

 

Best Regards,

 

Jim Nystrom

jnystrom@campbellap.com -

 

P  Please consider the environment before printing this e-mail

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Larry
Sent: Thursday, September 30, 2010 7:23 PM
To: materials-welding@googlegroups.com
Subject: [MW:7290] Electrode for cast steel

 

Hi,

 

Can anybody suggest a good electrode for cast steel?

 

No code applies, just common welding.

 

 

Thanks in advance.

 

 

 

Cheers,

Larry

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...