carry out PMI ie positive material identification this will help u a
lot
Muthu Barathi P
Sr. Manager QA / QC
AFCONS
On Wed, 22 Sep 2010 19:01:10 +0530 wrote
>Cehmical Analysis Can be done with the helpof Equipments like
Spectrometer or Spectromax to differentiate SS 304 and SS 316.
>
>--- On Thu, 16/9/10, soumya podder wrote:
>
>From: soumya podder
>Subject: [MW:7041] Method for checking SS Material
>To: materials-welding@googlegroups.com
>Date: Thursday, 16 September, 2010, 11:28 AM
>
>
Dear Sir ,
Pls explain how we check the material of SS like SS 316 or SS 304 .
>--
>Thanks & Regards
>
>Soumya Podder
>9099982514
--
>To post to this group, send email to materials-
welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>
Dear Sir,
Thanking You,
Honesty is the best Policy
With Warm Regards,
P Muthu Barathi
Mobile No:09967300544
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
carry out PMI ie positive material identification this will help u a
lot
Muthu Barathi P
Sr. Manager QA / QC
AFCONS
On Wed, 22 Sep 2010 19:01:10 +0530 wrote
>Cehmical Analysis Can be done with the helpof Equipments like
Spectrometer or Spectromax to differentiate SS 304 and SS 316.
>
>--- On Thu, 16/9/10, soumya podder
>
>From: soumya podder
>Subject: [MW:7041] Method for checking SS Material
>To: materials-welding@googlegroups.com
>Date: Thursday, 16 September, 2010, 11:28 AM
>
>
Dear Sir ,
Pls explain how we check the material of SS like SS 316 or SS 304 .
>--
>Thanks & Regards
>
>Soumya Podder
>9099982514
--
>To post to this group, send email to materials-
welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>
Dear Sir,
Thanking You,
Honesty is the best Policy
With Warm Regards,
P Muthu Barathi
Mobile No:09967300544
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments