Hi Manish,
You cannot do it as it is. Still SA106 Gr.B will not normally pass impact testing @ -45 Deg.C.
Thanks,
K.Rajagopal

On Tue, Sep 21, 2010 at 7:11 AM, Manish Mehta <mehtamanish81@googlemail.com> wrote:
Friends,

Can SA 333 Gr1 or G6 be substituted by SA106 Gr B with impact testing
at MDMT ?

Please share your knowledge.

Regards,
Manish

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...