ASTM A 262 Practice B is also called as streicher, Practice C is Huey, and Practice E is called as Strauss test. Type of test required and acceptance criteria should be stated by process designer depending on application
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
On Sat, Sep 18, 2010 at 4:02 PM, limesh M <limesh78@gmail.com> wrote:
Dear All,What is Huey test ?Huey test and intergranular corrosion test as per ASTM A262 are same or not ?How we are finding the Intergranular corrosion?What is the acceptance criteria?Regards,Limesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments