Skip to main content

Re: [MW:6959] Re: Duplex and Super Duplex Stainless Steel

Dear All,

Proposal came from client side as ER 2594 and E 2595-15.
What is the reason for using E2595-15 instead of E 2594 on this material for SMAW?at the same time they suggested ER 2594 for GTAW !!!  I have no idea.
Expecting some valuable comments in this regard.



Regards,

Limesh

On Fri, Sep 10, 2010 at 10:58 PM, vanchi <vanchinaths@gmail.com> wrote:
Dear Limesh,
SFA 5.4 E2594 electrode for Smaw and SFA 5.9 ER 2594 filler wire for
GTAW is used for welding UNS 32750.
Impact values are not specified by the code. It depends on the
consultants requirement. Upto minus 30degC you could use rutile base
electrode -16 or -17. incase you want to go lower down to minus 50degC
one should use basic -15 electrodes. For GTAW there is no issue. It
will pass minus 50degC. impact to be taken on the weld , notch
perpendicular to direction of welding.
incase u require further information mail it vanchi@vsnl.com

On Sep 9, 1:03 pm, limesh M <limes...@gmail.com> wrote:
> Dear All,
>
> Thank you for the valuable inputs.
>
> Construction codes: ASME B31.3 and welding code ASME SEC IX
>
> I want to weld ASTM A 790(UNS 32750) to ASTM A 790(UNS32750), ASTM A
> 928(UNS32750) to ASTM 928 (ASTM32750).Then ASTM ASTM A 790(UNS 32750) to
> ASTM A 928(UNS32750).What electrode and filler wire I have to select?
> Normally at what direction impact test doing on weld metal, ie, transverse
> or longitudinal or both direction? From where I can get the minimum charpy
> value required on impact test? I have reviewed ASTM standards, found minimum
> tensile and yield strength values, but couldn't find any minimum required
> impact value.
>
> Regards,
>
> Limesh
>
>
>
> On Sun, Sep 5, 2010 at 8:29 PM, limesh M <limes...@gmail.com> wrote:
> > Dear All,
>
> > What is the difference between Duplex and super duplex stainless
> > steel?
>
> > What is the P. No for duplex and super duplex stainless steel?
>
> > One of our duplex stainless steel PQR failed in impact test.What would
> > be the reason?
>
> > Thanks and Regards,
>
> > Limesh
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding-unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.- Hide quoted text -
>
> - Show quoted text -

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...