[MW:6882] selection of material Vs Chloride Content in water

In addition Mr Pradip's valuable inputs you may refer the attachments for guidelines. The actual corrosion is however a very complex process influenced by many different factors in combination.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pgoswami
Sent: Monday, September 06, 2010 8:42 AM
To: materials-welding@googlegroups.com
Subject: [MW:6878] MW:6877] Chloride Content

 

Prafulla,

Both 316 and 316L would work at the said 25 ppm chloride content level, provided the operating temperature does not exceed typically 20 deg C. Given a choice 316/316L (dual certified) grade should be the ideal material, otherwise, 316L shall  be used for piping. Welding consumable shall be of 316L grade  for all cases.

Following is an extract from :-Materials Selection for Refineries and Associated Facilities(A NACE publication)- by R A WHITE, Ex Materials and Corrosion Group Manager, Materials Quality Services Department,Bechtel Corporation

For materials selection, cooling water is normally categorized as either freshwater or salt water.Austenitic SS's are  used in freshwater. For freshwater application, to avoid pitting, type 304 (UNS S30400) SS is normally limited to services in which the chloride ion concentration is at a maximum of 100 ppm, and type 316 SS is limited to services in which the chloride ion is a maximum of 500 ppm.( The designer may have to apply his/her conservatism to this number depending on plant design and operating conditions). 

The relative pitting and crevice corrosion resistance of SS alloys can be approximated by the following equation:-PRE = %Cr + 3.3%M0 + 16%N.

Theoretically, pitting will not occur (regardless of the chloride ion concentration) if the temperature in degrees Celsius is limited to 5°C plus 7 times the molybdenum content. Thus, for a 2% molybdenum alloy (e.g.,  316 SS), the limit would be typically : 19deg C

When austenitic SS's are required, low carbon or stabilized grades should be  used to avoid intergranular corrosion.

For salt water application:- theoretically, austenitic SS's can be used in salt water if the velocity exceeds 3 ft/s (0.9 m/s). But in stagnated water different scenario may arise.Experience has shown that stagnant conditions will always occur in a salt water system resulting in rapid pitting (average penetration rates are on the order of 70 mpy ). Typically for salt water application, the  new super SS's that are high in molybdenum and resistant to seawater attack  and duplex stainless steels are being used more frequently in cases in which seawater attacks from both side

I hope this clarifies your query.

Thanks.

Pradip Goswami,P.Eng.

Welding & Metallurgical Engineer/Specialist

Ontario Power Generation Inc.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Praphulla Phirke
Sent: Sunday, September 05, 2010 12:46 PM
To: materials-welding@googlegroups.com; 'Kisan Gamane'
Subject: RE: [MW:6877] Chloride Content

Hi Kisan

Thanks for your help but I want to select either SS 316 or SS 316 L… So can you guide me up to what limit SS 316 is OK and beyond which its not?

 

Thanks & Regards

Praphulla

praphulla.dp@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kisan Gamane
Sent: Sunday, September 05, 2010 5:41 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6873] Chloride Content

 

Dear Praphulla

I think material u can used 316 or 316 L. But a cooling water which will enter inside the plumblene ie. to be cloride contain up to 25 ppm.

On Sat, Sep 4, 2010 at 11:32 PM, Praphulla Phirke <praphulla.dp@gmail.com> wrote:

Dear All, Can someone guide me where I can get the details to select the materials according to chloride content in water?

 Recent in our project customer has asked us to choose the material as per the chloride content..whether to go for SS 316 or 316L.

 What is the limit for SS 316  & 316 L considering the chloride content in the cooling water?

 Thanks & Regards

Praphulla


Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...