Appreciate if you could provide me some information on the issue, During a PQR, manufacturer has used electrode F6A0-EM12 to weld plates A516 Gr. 65, welding procedure is SAW. Below is the comparison, between the tensile strength of the electrode,
comparison table
WELDING FLUX F6A0 PLATE flux certificate(see attachment) Strength of the plate material
REFER TO SFA 5.17 ASTM A516, GR65 test result Test Result
Tensile Tensile tensile tensile
60,000~80,000 psi 65000~85,000 psi 72289 psi (500MPa) 68875 psi (475 Mpa)
Our client says that the selected electrode is not suitable for Gr. 65c plates. Is it correct?They say that the electrode shall be selected considering the minimum strength ( for this electrode minimum strength is 60, 000 PSI), and therefore it is not suitable for a plate with minimum strength value equal to 65000 PSI .
As you can see in the above table tensile test value for the electrode is 72289 PSI, but still the client is not ready to accept the use of this electrode.
Please advise.
Regardsa
MS
______________________________________________________
CONFIDENTIALITY NOTICE: This electronic mail transmission may contain information that is confidential, privileged, proprietary, or otherwise legally exempt from disclosure and is intended only for the use of the recipient named above. We do not waive confidentiality in the event this mail was transmitted wrongly. If you have received this communication in error, and are not the intended recipient, you are hereby notified that you are prohibited from reading, printing, copying, or disseminating this message, any part of it, or any of the attachments it may carry. If you have received this message in error, please destroy all electronic and paper copies and notify the sender immediately of the inadvertent transmission. We would like to advise you that we would not waive any of our privilege for taking action against you in the event the confidentiality of this message has been compromised. Thank you for your cooperation
________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
With Best Regards
B.Vaithiyanathan --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments