Skip to main content

Re: [MW:6578] Difference welder and welding operator

Hi
 
As per AWS D1.1 , Tack welder have  to qualified.
 
As per ASME Sec IX , tack welder has to be qualified by fillet weld qualification.
 
Rgds,
 
K.Babu
Singapore
 
----- Original Message -----
From: skrie85
Sent: Wednesday, August 18, 2010 4:58 PM
Subject: Re: [MW:6562] Difference welder and welding operator

Tack welder need to qualify or not?


From: Karthik <karthik6684@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Wed, August 18, 2010 3:48:47 PM
Subject: Re: [MW:6556] Difference welder and welding operator

Hi,

Please find below the definition of welder and welding operator and tack welder.

WELDER:

A welder is one who performs a manual or semiautomatic welding operation.This includes welding with torch,gun or electrode holder held and manipulated by hand.Part motion devices and manually controlled filler metal feeders may be used.Semi automatic welding is manual welding with equipment that automatically controls one or more of the welding conditions,usually filler wire feed.A welder would commonly perform shielded metal arc,gas metal arc,and flux cored arc welding.


WELDING OPERATOR:

A welding operator is one who operates adaptive control,automatic,mechanized,or robotic welding equipment.Automatic welding is with equipment that reqires occasional or no observation of the welding and no manual adjustments of the welding controls.Mechanized welding is with equipment that requires manual adjustment of the equipment controls in response to visual observation of the welding,with torch,gun or electrode holder held by a mechanical device.Most submerged arc welding setups would fit in to this category.


TACK WELDER:

A tack welder is a fitter,or someone under the direction of a fitter,who tack welds parts of a weldment to hold them in proper alignment until the final welds are made.


Thanks & Regards,


(Karthik)


Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 8/18/10, skrie85 <skrie85@yahoo.com> wrote:

From: skrie85 <skrie85@yahoo.com>
Subject: [MW:6554] Difference welder and welding operator
To: materials-welding@googlegroups.com
Date: Wednesday, August 18, 2010, 12:33 PM

Dear all,

What difference "welder" and "welding operator" stated in ASME IX?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...