Thanks pradeep
In this circumstance could you please elaborate on the extra precautions to be taken during welding?
Regards
Hrishi

-- --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
In this circumstance could you please elaborate on the extra precautions to be taken during welding?
Regards
Hrishi
Sent on my BlackBerry® from Vodafone Essar
From: "pgoswami" <pgoswami@quickclic.net>
Sender: materials-welding@googlegroups.com
Date: Wed, 11 Aug 2010 13:39:29 -0400
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:6449] MW:6444- F91 vs F9 grade flanges
Hrishi,
Pleas see the extract from SA182,FYI info. I think your supplier got caught between F91 and F9 specification. V to the level of 0.19% can affect weldability significantly. Advice would be to perform a wet chemical analysis on the flanges,if the results are consistent with the test certificate then take the matter with client and seek their concurrence.
The supplied material look to be closer to the chemistry of of 91 steel.If so please note that a change from F9 to F91could be quite significant.
Thanks.
Pradip Goswami,P.Eng.
Welding & Metallurgical Engineer/Specialist
Ontario Power Generation Inc.
Email-pgoswami@sympatico.ca,
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of K.M Hrishikesan
Sent: Wednesday, August 11, 2010 10:09 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6444] F91 vs F9 grade flanges
Sent: Wednesday, August 11, 2010 10:09 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6444] F91 vs F9 grade flanges
Dear Raghuram & Jignesg Rana
- The PMI result is as follows: Cr-8.66%, Mo-0.96% and V-0.19%
- There is no Cb content
- Intended service of the line is Coke Drum Overhead vapour and Coke drum Blow down vapour line.
Regards
Hrishi
On Wed, Aug 11, 2010 at 4:36 PM, <jignesh.rana@linde-le.com> wrote:
Dear Hrishi,Can you share PMI results ?What was the referent standard used ?Please inform end application of the product also.With Best Regards,Jignesh R RanaManager - QA & QCLinde Engineering India Pvt. Ltd.38, Nutan Bharat Society, Alkapuri, Vadodara 390007, IndiaTel.: +91 265 3056789, Fax: +91 265 2335213 , Mobil: +91 90999 86019This e-mail is confidential. If you are not the intended recipient, please notify us immediately. You should not disclose its contents to any other person nor use it for any purposes.
| hrishikm07@gmail.com Sent by: materials-welding@googlegroups.com 11-08-10 05:18
|
|
Hi
I have some LA flanges certified as F9 grade as per MTC and TPI certificate. But when I conducted PMI using NITON-XRF machine I have observed presence of Vanadium slightly lower than F91 requirements in some of them.
My query is
If it is of F9 why there is Vanadium presence?
Can I accept it as F9 grade?
Thanks
Hrishi
Sent on my BlackBerry® from Vodafone Essar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments