Skip to main content

Re: [MW:6424] Qualification of pipe

SKRIE,
 
You didn't mentioned the process and consumable used,F Number of welding consumable is an important parameter to determine welders range of qualification.Anyhow as per available information ,following are the answers.
 
1) I have qualified for welding pipe 2" (60.3mm OD) material P-No.1 to P-No.1.
 
Do I qualified for welding
 
a) pipe 6" (168.3mm OD)
Yes,Refer QW 452.3

b) material P-No.8 to P-No.8
Yes,Refer QW 423.1

c) pipe P-No.10H to P-No.10H with 2" (OD).
 
Yes,Refer QW452.3 and QW 423.1
 
2) If we welding pipe, the qualification base on OD pipe or thickness pipe?
 
Welder qualification based on Pipe diameter,Pipe thickness.Another important parameter is F Number of welding consumable.
 
Thanks.

On Mon, Aug 9, 2010 at 4:40 PM, N VENKATESWARA PRASAD <weldengr.velosi@gmail.com> wrote:
Hi,
 
The F no will change only if use SMAW.  But if you have used GTAW then Fno will not change and as you are going to purge which not essential vairable for welder qualificiaton.  Deletion of purging is essential vairable, addtion of purging is not essential variable.
 
Regards
 
N.V. PRASAD

On Mon, Aug 9, 2010 at 12:07 PM, Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com> wrote:
If you speak about WPS according to ASME IX then under the conditions you wrote, your welding conditions are qualified for pipe 6" according to QW-452.3
the P-No.1 to P-No.1 can not  qualify  P-NO.8 to P-No.8 as per QW-424.1 and also can not qualify P-NO.8 to P-No.8 as per QW-424.1

If you speak about WPQ according to ASME IX then under the conditions you wrote, your welding conditions are qualified for pipe 6" according to QW-452.3
the P-No.1 to P-No.1 can qualify  P-NO.8 to P-No.8 as per QW-424.1 and also can qualify P-NO.10H to P-No.810H as per QW-423.1



1) I have qualified for welding pipe 2" (60.3mm OD) material P-No.1 to P-No.1.

Do I qualified for welding
a) pipe 6" (168.3mm OD)
b) material P-No.8 to P-No.8
c) pipe P-No.10H to P-No.10H with 2" (OD).

2) If we welding pipe, the qualification base on OD pipe or thickness pipe?

Thanks.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Welder's Helper
 
Never bend my head infront of anyone other than GOD the almighty.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...