I think, you have to qualify the process using WPS(Welding Procedure Specification, ASME Section IX) and its test PQR (Pocedure Qualification Record). If the procedure pass the test you can apply it.
Regards,
jml
--
Jorge Mejia Lema.
Especialista IV Mecánico.
Gerencia Tanques.
PBX: +57 (1) 3215801 Ext. 4094
FAX: +57 (1) 3215913
Cell: 3174793091
Carrera 11 No.71-73 Piso 10
ITANSUCA PROYECTOS DE INGENIERIA Ltda.
Bogotá, Colombia, Sur América
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Regards,
jml
2010/8/9 Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com>
--Please i hope to know if any body works in circumferential welds in tanks with 6mm in thickness and the material is SA-283 Gr.B can i use one one pass full penetration using SAW in square joint with NO gapplease refer to the reference
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Jorge Mejia Lema.
Especialista IV Mecánico.
Gerencia Tanques.
PBX: +57 (1) 3215801 Ext. 4094
FAX: +57 (1) 3215913
Cell: 3174793091
Carrera 11 No.71-73 Piso 10
ITANSUCA PROYECTOS DE INGENIERIA Ltda.
Bogotá, Colombia, Sur América
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments