Some clients especify what kind of NDT and the percentaje that has to be aplied for headers , here in Ecuador many accidents have happened in hidrostatic tests therefore a common practice is RT/UT for girth welds and DPT weld-thread o'lets, and  no one header can be used more than three times, of couse the header has to be tested before the pipeline, in every test

BR


Date: Sat, 7 Aug 2010 15:19:14 +0530
Subject: Re: [MW:6358] Hydrotesting of pipeline
From: rajeevarora007@gmail.com
To: materials-welding@googlegroups.com

for safety point of view and for the confirmation of the weld quality you can adopet the any NDT method according to the requirement like RT having the record and UT no record  ( RT and UT  can check the quality of complete weld ) and DPT is only for the surface defect.
 
it will be advicable to have the RT and DPT test for the weld of header rest depand on the procedure or specification.

On 7 August 2010 12:42, sumit jaura <sumit.jaura@gmail.com> wrote:
Dear all,

Can anyone suggest that whether it is must to have radiography of all
flanges and nipples on test header for hydrotesting?

or we can only allow by ut or dpt only.

Sumit ,

P. engineer,

Worleyparsons

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards

Rajeev Arora




"DON'T LET SOMEONE BECOME A PRIORITY IN YOUR LIFE...
WHEN YOU ARE JUST AN OPTION FOR THEM....."

 SO , Always keep in mind that......

DON'T GO THE WAY LIFE TAKES YOU,
TAKE THE LIFE THE WAY YOU GO,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...