Yes, Need not be a U2 stamp holder.
arun

On Wed, Aug 4, 2010 at 10:02 PM, <george.dilintas@gr.bureauveritas.com> wrote:

R stamp holder yes but not necessarily U2 stamp holder


  From: Arunachalam A [arunvani@gmail.com]
  Sent: 04/08/2010 21:35 ZE5B

  Subject: Re: [MW:6309] Asme Stamps according section VIII division 2


Any repairs to U2 stamped vessel shall be as follows:
1. Any repairs shall be done by an R-Stamp holder, who should also have U2 stamp for new construction.
2. R-Stamp holder shall prepare a repair plan which shall be in conformance with UDS, Manufacturer's design report and MDR.
3. Repair plan shall be sent to an Registered Professional Engineer for his certification.
4. Once his certification is completed, the repair plan along with Drawing/UDS/Manfacturer's design report/MDR shall be submitted to ASME Authorized Inspector, with whom the R-Stamp holder has an Inspection agreement.
5. AI inspects the vessel and agrees with repair plan.
6. R-Stamp holder Carries out repair.
7. Carries out NDE and /Or hydrostatic set as per Repair plan.
8. After AI accepts the repair completion inspection, he authorizes R-Stamping.
9. R-Stamp holder prepares, and gets it certified by AI.

arun

On Wed, Aug 4, 2010 at 3:56 AM, guttemberg.souza <guttemberg.souza@uol.com.br> wrote:
Dear All,

Who can help me about a case regarding a pressure vessel stamped as "U2" which was manufactured, approved and shipped to the company i work for. But during the receiving inspection, in order to fit it to its final position, and according to internal inspection, some defects have been revealed on the visual weld inspection on the root of one of its nozzle like undercuttings, lack of fusion and concavity. We asked for the x-ray film to the manufacturer and they have sent to us but the result was approved. Then we have decided to perform another x-ray  on that joint to confirm the manufacturer x-ray, using the same x-ray techinique and the result revealed porosities out of ASME VIII div 2 requirements. So, in this case, if we decide to repair this joint, would we need to classify the vessel again ?

Best regards,


Guttemberg Souza

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...