Re: [MW:6307] Asme Stamps according section VIII division 2

Dear Guttemberg Souza
You can not carry out any repair on the vessel, as it is ASME stamped vessel. Only ASME authorized shop can do the repair with application of R stamp. Again this will inspected by ASME authorized inspector. I suggest you carefully review the Manufacturer's Data Report of the vessel, there you will find parameters including RT done,during design & fabrication of the vessel. You can consult with agencies providing ASME inspection services viz LR insurance, Bureau Veritas, ABS etc for any advice.
 
Mhaskar Aly
Kuwait
 
 

From: guttemberg.souza <guttemberg.souza@uol.com.br>
To: materials-welding@googlegroups.com
Sent: Wed, August 4, 2010 1:26:31 AM
Subject: [MW:6299] Asme Stamps according section VIII division 2

Dear All,

Who can help me about a case regarding a pressure vessel stamped as "U2" which was manufactured, approved and shipped to the company i work for. But during the receiving inspection, in order to fit it to its final position, and according to internal inspection, some defects have been revealed on the visual weld inspection on the root of one of its nozzle like undercuttings, lack of fusion and concavity. We asked for the x-ray film to the manufacturer and they have sent to us but the result was approved. Then we have decided to perform another x-ray  on that joint to confirm the manufacturer x-ray, using the same x-ray techinique and the result revealed porosities out of ASME VIII div 2 requirements. So, in this case, if we decide to repair this joint, would we need to classify the vessel again ?

Best regards,


Guttemberg Souza

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...